Nylon woven bag Granulation Trial Run

Nylon woven bag granulation Trial Run

  1. Shredding: The nylon bags are shredded into smaller pieces.
  2. Прање: The shredded nylon is washed to remove any impurities.
  3. Melting: The clean nylon shreds are melted down.
  4. Extruding: The molten nylon is then extruded through a die to form long strands.
  5. Cooling: These strands are cooled, typically in a water bath.
  6. Сечење: Once cooled, the strands are cut into pellets.